材料 Material Group |
合金名稱 Alloy Name |
密度Density |
含碳量Carbon Content |
抗拉強度Tensile Strength |
伸長率Elongation |
硬度Hardness |
磁性Magnetic response |
合金鋼 Alloy Steel |
4605 (As-Sintered) |
7.5 |
0.6% max. |
440 |
15 |
HRB 70 ~ 80 |
Average |
4605 (Quenched & Tempered) |
7.5 |
0.6% max. |
1655 |
2 |
HRC 48 ~ 52 |
Average |
|
4605 Modified |
7.5 |
0.6% max. |
1800 |
8 |
HRC 48 ~ 53 |
Average |
|
4350 (As-Sintered) |
7.5 |
0.6% avg. |
440 |
15 |
HRB 100 ~ 105 |
Average |
|
4350 (Quenched & Tempered) |
7.5 |
0.6% avg. |
1655 |
2 |
HRC 40 ~ 55 |
Average |
|
4350 Modified |
7.5 |
0.6% avg. |
1800 |
9 |
HRC 40 ~ 55 |
Average |
|
沃斯田鐵不鏽鋼Austenitic Stainless Steel |
316L |
>7.5 |
0.03% |
500 |
18 |
HRB 50 ~ 60 |
N/A |
304L |
>7.5 |
0.03% |
500 |
15 |
HRB 50 ~ 60 |
N/A |
|
肥粒鐵不鏽鋼 Ferritic Stainless Steel |
430 |
0.12% |
Average |
||||
麻田散鐵不鏽鋼Martensitic Stainles Steel |
420 |
7.2 |
>0.15% |
1200 |
1~2 |
HRC 46 ~ 50 |
Average |
440C |
7.6 |
0.95~1.2% |
800 |
< 1% |
HRC 50 ~ 55 |
Average |
|
析出硬化型不鏽鋼precipitation Harding Stainless Steel |
17-4PH (As-Sintered) |
7.5 |
<0.07% |
900 |
6 |
HRC 23 ~ 26 |
LOW |
17-4PH (Heat-Treated) |
7.5 |
<0.07% |
1190 |
5 |
HRC 33 ~ 45 |
LOW |
|
軟磁材料 Soft Magnetic Materials |
1010 |
7.6 |
<0.1% |
700 |
12 |
HRB 70 ~ 80 |
Good |
1008 |
7.6 |
<0.08% |
700 |
12 |
HRB 70 ~ 80 |
Good |
|
工具鋼 Tool Steel |
SKD-11 (D2) (Heat-Treated) |
7.7 |
1.50% |
800 |
< 1% |
HRC 58 ~ 63 |
Average |
鎢 Tungsten |
鎢合金 Tungsten Alloy |
9~15 |
>500 |
||||
碳化鎢 Tungsten Carbide |
11 |
6.13% |
HRC 72 ~ 75 |
||||
鈦 Titanium |
純鈦 CP4 |
4.7 |
550 |
15 |
HRB 100 |
||
64鈦 Ti-6Al-4V |
4.5 |
|
|
|
|
|